How Tempered Glass Is Made: The Complete Manufacturing Process

Tempered glass is one of the most widely used safety glazing products in construction. But how exactly is it made? We walk through the full manufacturing process from raw glass to finished tempered panel.

Rez Glass Industries 2026-03-01

What Is Tempered Glass?

Tempered glass — also known as toughened glass — is a type of safety glass processed through a controlled thermal or chemical treatment to increase its strength. When broken, it shatters into small, blunt granular chunks rather than sharp jagged shards, significantly reducing the risk of injury.

Step 1: Cutting the Raw Glass

The process begins with standard annealed (float) glass, which is cut to the required dimensions using automated CNC cutting tables. Precision is critical at this stage because tempered glass cannot be cut or drilled after the tempering process — all holes, notches, and edge work must be completed beforehand.

Step 2: Edgework and Drilling

Once cut, the glass undergoes edge finishing — polishing, seaming, or beveling — depending on the application. Any required holes for hardware (like standoffs or hinges) are drilled using diamond-tipped bits. All dimensions are verified before proceeding.

Step 3: Washing and Inspection

The glass is thoroughly washed to remove any debris, oil, or contaminants that could cause optical distortions or defects during heating. Automated washers use deionized water and soft rollers to ensure a clean surface.

Step 4: The Tempering Furnace

The cleaned glass enters the tempering furnace, where it is heated to approximately 620–680°C (1150–1260°F) — well above the glass transition temperature. The glass travels through the furnace on ceramic rollers, which can sometimes leave faint roller wave distortions visible in certain lighting conditions.

Step 5: The Quench — Rapid Cooling

Immediately after exiting the furnace, the glass enters the quench section, where powerful air jets rapidly cool the surface of the glass. The outer surfaces cool and solidify much faster than the inner core, which is still cooling and contracting. This creates a permanent state of compression on the surface and tension in the core — this differential stress is what gives tempered glass its strength.

Step 6: Inspection and Quality Control

After tempering, each panel is inspected for optical clarity, bow, warp, and surface defects. A polarized light test can detect internal stress patterns. Tempered glass is also tested to ensure it meets CSA and ASTM standards for safety glazing.

Why Tempered Glass Is Stronger

The compressive stress built into the surface makes tempered glass approximately four times stronger than standard annealed glass of the same thickness. To break through the surface, an impact force must first overcome the surface compression before the tension inside can cause failure.

Applications

Tempered glass is used in shower enclosures, glass railings, entry doors, sidelites, office partitions, shelving, table tops, and any application where human impact is a concern. Building codes across Canada require tempered or laminated glass in specific locations for occupant safety.

At Rez Glass

We temper glass in-house using our state-of-the-art tempering furnace at our Mississauga facility. All tempered glass is produced to CSA and ASTM standards with fast 2–7 day lead times. Contact us for pricing and specifications.